since 1966 Metal fabrication Radolfzell · Germany +49 7732 3511 Sign in
Language: EN

Materials guide · V2A, V4A and duplex compared Which stainless steel suits your component?

The choice of material decides whether a component lasts ten years or shows surface rust after two – and whether you spend more money than necessary. Here is what we have learned at the workbench in six decades of stainless steel fabrication.

Kemmer logo on brushed stainless steel

The short answer

1.4301 (V2A) is the standard for indoor structures, racks, panels and anything that does not come into contact with chlorides. 1.4404 and 1.4571 (V4A) additionally contain molybdenum and are the right choice for salt, chlorides, acids, cleaning agents, food and outdoor use. 1.4462 (duplex) has about twice the yield strength of the austenitic grades and considerably higher chloride resistance – useful for high mechanical loads or aggressive media.

Rule of thumb: in dry indoor areas 1.4301 is enough. As soon as water, salt or cleaning chemicals come into play, use V4A. For boats in salt water, 1.4571 is the classic.

Direct comparison

The four grades we process most often

We keep all four in stock as sheet, tube or profile; the cut-to-size editor prices sheets in 1.4301, 1.4404 and 1.4571 right away. The figures are guide values from the relevant standards – what counts is always the mill certificate of the specific batch.

Comparison of the common stainless steel grades
Property 1.4301 1.4404 1.4571 1.4462
Steel name X5CrNi18-10 X2CrNiMo17-12-2 X6CrNiMoTi17-12-2 X2CrNiMoN22-5-3
Common designation V2A, AISI 304 V4A, AISI 316L V4A, AISI 316Ti Duplex 2205
Microstructure austenitic austenitic austenitic austenitic-ferritic
Chromium / nickel 17.5–19.5 % / 8–10.5 % 16.5–18.5 % / 10–13 % 16.5–18.5 % / 10.5–13.5 % 21–23 % / 4.5–6.5 %
Molybdenum no approx. 2 % approx. 2 % approx. 3 %
PREN (guide value) approx. 18 approx. 24 approx. 24 approx. 35
Yield strength Rp0.2 approx. 230 N/mm² approx. 240 N/mm² approx. 240 N/mm² approx. 460 N/mm²
Tensile strength Rm 540–750 N/mm² 530–680 N/mm² 540–690 N/mm² 640–840 N/mm²
Magnetic no (slightly after forming) no (slightly after forming) no (slightly after forming) yes
Chlorides / salt water unsuitable good good very good
Forming & bending very forgiving forgiving forgiving higher forces, more springback
Welding straightforward straightforward straightforward, titanium-stabilised heat input must be right
Material cost low medium medium to high high
Typical for racks, panels, indoor use food, pharma, chemicals boatbuilding, process engineering highly stressed containers

PREN = Pitting Resistance Equivalent Number, calculated as %Cr + 3.3 × %Mo + 16 × %N. The higher the value, the more resistant to pitting. Composition to EN 10088-1, strength to EN 10088-2 for cold-rolled sheet (duplex: hot-rolled) – what counts is the 3.1 inspection certificate of the material.

For bending, our editors use the same inside radius and minimum flange length for all grades; stainless steel, however, needs almost three times the press force of aluminium. The values for each sheet thickness are in the bending chart.

Decision guide

Which material for which application?

Go through the questions from top to bottom. As soon as one applies, you have your answer.

Question 1

Does the part come into contact with salt water, road salt or chlorides?

Then at least 1.4404 or 1.4571. In a chloride environment 1.4301 develops pitting – you don't see it immediately, but after one or two seasons. For boats in salt water and for fittings permanently exposed to spray, 1.4571 is the classic.

Question 2

Is it cleaned daily with aggressive agents?

In food, beverage and pharmaceutical plants the cleaning chemicals are often more demanding than the product itself. Here too, 1.4404 is a sensible minimum – with welds cleanly ground flush and pickled.

Question 3

Does the component have to take high forces or be thinner?

1.4462 has about twice the yield strength of the austenitic grades. That allows thinner walls with the same load-bearing capacity – which partly offsets the higher material price.

Question 4

None of these applies?

Then use 1.4301. It is cheaper, more readily available, easier to bend and to weld. Choosing a more expensive material “to be on the safe side” costs money without any benefit.

A special case: temperature

With permanently raised temperatures and long dwell times in the critical range, intergranular corrosion can occur in unstabilised grades. Low-carbon variants such as 1.4404 or titanium-stabilised ones such as 1.4571 help against this. If your component gets warm permanently, tell us the temperature – then we clarify this in advance.

From practice

Why stainless steel rusts after all

In the vast majority of cases that reach us, it is not the material that is to blame but the processing. These four causes cover almost everything.

1. Extraneous rust from contact with carbon steel
If stainless steel and ordinary steel are worked with the same tools, brushes or grinding discs, iron particles get onto the surface. These particles rust – and it looks as if the stainless steel itself were rusting. That is why brushes, grinding discs and tools that have been used on carbon steel do not belong on stainless steel.
2. Heat tint that was not removed
Welding leaves bluish-brown heat tint next to the weld. In this zone the protective passive layer is damaged. Leave it, and you will get corrosion exactly there later. Pickling and passivation restore the protection – that is not a cosmetic luxury but a technical necessity.
3. Crevices and dead corners
Liquid stands in narrow crevices, under supports and in welds that are not fully penetrated. That is where crevice corrosion develops, even in high-grade materials. The design solution is fully penetrated welds, inside radii instead of sharp corners and a slope to the drain.
4. The wrong material in the wrong place
1.4301 in a swimming pool, on the coast or near road salt is the most common classic. The material is perfectly fine – just not for this environment.

Frequently asked questions

On stainless steel grades

What do V2A and V4A mean?

The names originally come from the development history at Krupp and stand for “Versuchsschmelze Austenit” (experimental austenite melt). In everyday language, V2A today means grade 1.4301 without molybdenum, V4A the molybdenum-alloyed grades 1.4404 and 1.4571. They are not standardised material designations – the quote and the drawing should always state the material number.

Is stainless steel magnetic?

The austenitic grades 1.4301, 1.4404 and 1.4571 are practically non-magnetic as delivered. Cold forming – bending, rolling or deep drawing – can partly transform the microstructure, so that a magnet sticks slightly. That is normal and not a sign of inferior material.

Duplex 1.4462, on the other hand, is clearly magnetic because half of it consists of ferrite.

How can I tell whether an existing part is V2A or V4A?

Reliably only by a material analysis. The magnet test says nothing, because both grades are austenitic. If you have a sample part reproduced and the material is unknown, we go by where it was used: where the part was installed and what it had to withstand usually reveals more than any quick test.

Why does stainless steel rust after angle grinding or welding?

Usually for one of two reasons: iron abrasion from cutting discs, brushes or tools previously used on ordinary steel (extraneous rust), or heat tint after welding and heating – there the protective chromium oxide layer is disturbed. Remedy: use abrasives for stainless steel only and pickle and passivate the surface after welding.

1.4404 or 1.4571 – what is the difference?

Both are V4A with molybdenum and almost equally resistant to chlorides, acids and salt. 1.4404 (316L) is low-carbon, 1.4571 (316Ti) is stabilised with titanium – both prevent intergranular corrosion of the material next to the weld. 1.4404 polishes better and is therefore preferred in food and pharmaceutical areas; 1.4571 is widespread in container and plant construction and somewhat stronger at higher temperatures.

Is stainless steel compatible with ordinary steel?

With permanent contact and moisture, the unalloyed steel corrodes faster than on its own – that is galvanic corrosion; the stainless steel itself is not damaged. Outdoors and in wet areas the materials are therefore separated with plastic washers or sleeves. A second risk is extraneous rust: iron particles from tools previously used on carbon steel rust on the stainless steel surface.

Unsure about the choice of material?

In the request form, choose “Not sure – please advise” (in the German form: „Weiß ich nicht – bitte beraten“) and describe the place of use. We suggest the right material – with reasons. We reply in German or English.

Free, no-obligation quote Reply within 24–48 hours on working days

Call Quote