since 1966 Metal fabrication Radolfzell · Germany +49 7732 3511 Sign in
Language: EN

Quality levels · Ra values, ISO 2768, ISO 5817 How smooth, how accurate, how cleanly welded?

Every extra level costs grinding, measuring and inspection time. Here is what Ra values, tolerance classes and quality levels mean – so that the drawing states what your part needs, and no more.

Stainless steel container unit, visible surfaces under protective film

In brief

Surface: Ra is the mean deviation of the surface from its centre line in micrometres – the smaller, the smoother. Cold-rolled stainless steel sheet 2B is usually Ra 0.1 to 0.5 µm, a ground finish with grit 240 about 0.3 to 0.6 µm; for surfaces in contact with food, EHEDG recommends at most Ra 0.8 µm. Tolerance: where no dimension is toleranced individually, the general tolerance applies – usually ISO 2768-m, i.e. ±0.3 mm at 100 mm. Weld: ISO 5817 divides welds into the quality levels B (stringent), C (intermediate) and D (moderate).

Tighter values are best specified only on the surfaces, dimensions and welds that really need them – everything else is covered by the general note in the title block.

Surface quality

What the Ra value measures

Ra (arithmetic mean roughness) is the mean of the profile's deviations from its centre line, measured over a defined length. Rz, the mean roughness depth, is always larger for the same surface – depending on the process a multiple of Ra. On the drawing the value is given at the surface texture symbol to ISO 21920-1 (formerly ISO 1302).

Three roughness profiles at the same scale Profile with Ra 3.2 µm with regular grooves, profile with Ra 0.8 µm irregular and considerably flatter, profile with Ra 0.2 µm almost smooth. The band shows plus and minus Ra around the centre line. Ra 3.2 µmturned or milled, finish cut – feed marks +Ra−Ra centre line Ra 0.8 µmground – limit for food contact (EHEDG) Ra 0.2 µmbright annealed (2R), finely ground or polished
Three calculated profiles at the same scale: evaluation length 4 mm, vertically exaggerated about 35 times. The light band extends from −Ra to +Ra.

Ra guide values by surface and process

What a surface achieves depends on material, tool, belt and initial condition – the bars are guide values from the technical literature and from material manufacturers, not a promise. We grind and brush in-house to the required grit and pickle and passivate welds (surface treatment); other surfaces on request.

Ra guide values by surface and process, logarithmic scale Bars from–to in micrometres. Stainless steel sheet: 2R bright annealed 0.05 to 0.2; 2B cold-rolled 0.1 to 0.5; ground, grit 320 0.2 to 0.4; ground, grit 240 0.3 to 0.6; ground, grit 120 0.6 to 1.2; electropolished 0.1 to 0.4. Machining: grinding 0.1 to 1.6; fine turning, fine milling 0.4 to 1.6; reaming 0.8 to 3.2; finish turning and milling 1.6 to 6.3; drilling 3.2 to 12.5; sawing 6.3 to 25. Line at 0.8 µm: EHEDG recommendation for product contact surfaces. 0.025 0.025 0.05 0.05 0.1 0.1 0.2 0.2 0.4 0.4 0.8 0.8 1.6 1.6 3.2 3.2 6.3 6.3 12.5 12.5 25 25 Ra in µm Stainless steel sheet: as delivered and ground 2R bright annealed 2R bright annealed: Ra 0.05 to 0.2 µm 0.05–0.2 2B cold-rolled 2B cold-rolled: Ra 0.1 to 0.5 µm 0.1–0.5 Ground, grit 320 Ground, grit 320: Ra 0.2 to 0.4 µm 0.2–0.4 Ground, grit 240 Ground, grit 240: Ra 0.3 to 0.6 µm 0.3–0.6 Ground, grit 120 Ground, grit 120: Ra 0.6 to 1.2 µm 0.6–1.2 Electropolished Electropolished: Ra 0.1 to 0.4 µm 0.1–0.4 Machining and sawing Grinding Grinding: Ra 0.1 to 1.6 µm 0.1–1.6 Fine turning, fine milling Fine turning, fine milling: Ra 0.4 to 1.6 µm 0.4–1.6 Reaming Reaming: Ra 0.8 to 3.2 µm 0.8–3.2 Finish turning, milling Finish turning, milling: Ra 1.6 to 6.3 µm 1.6–6.3 Drilling Drilling: Ra 3.2 to 12.5 µm 3.2–12.5 Sawing Sawing: Ra 6.3 to 25 µm 6.3–25 EHEDG ≤ 0.8
Logarithmic scale in the preferred series of Ra values. Line at 0.8 µm: EHEDG recommendation for product contact surfaces.
Values as a table
Ra guide values in µm
Surface, processRa from – toGroup
2R bright annealed0.05 – 0.2sheet
2B cold-rolled0.1 – 0.5sheet
Ground, grit 3200.2 – 0.4sheet
Ground, grit 2400.3 – 0.6sheet
Ground, grit 1200.6 – 1.2sheet
Electropolished0.1 – 0.4sheet
Grinding0.1 – 1.6machining, sawing
Fine turning, fine milling0.4 – 1.6machining, sawing
Reaming0.8 – 3.2machining, sawing
Finish turning, milling1.6 – 6.3machining, sawing
Drilling3.2 – 12.5machining, sawing
Sawing6.3 – 25machining, sawing

General tolerances

ISO 2768: what applies without an individual tolerance

If the title block says “ISO 2768-mK”, every dimension without its own tolerance is subject to class m (medium) for lengths and angles according to part 1 and class K for form and position according to part 2. Tighter dimensions are given individually at the dimension – as a deviation (±0.1), as a fit (H7) or as a geometrical tolerance in a frame.

General tolerance to ISO 2768-1 for a dimension of 100 mm Class f (fine) plus or minus 0.15 mm; class m (medium) plus or minus 0.3 mm; class c (coarse) plus or minus 0.8 mm; class v (very coarse) plus or minus 1.5 mm. -1.5 -1 -0.5 100 mm +0.5 +1 +1.5 Deviation in mm ffine ISO 2768-f at 100 mm: ±0.15 mm ±0.15 mmedium ISO 2768-m at 100 mm: ±0.3 mm ±0.3 ccoarse ISO 2768-c at 100 mm: ±0.8 mm ±0.8 vvery coarse ISO 2768-v at 100 mm: ±1.5 mm ±1.5
Tolerance zone of the four classes at a nominal size of 100 mm (range over 30 to 120 mm).
ISO 2768-1: permissible deviations for linear dimensions in mm
Linear dimension in mmf finem mediumc coarsev very coarse
0.5 to 3±0.05±0.1±0.2–
over 3 to 6±0.05±0.1±0.3±0.5
over 6 to 30±0.1±0.2±0.5±1
over 30 to 120±0.15±0.3±0.8±1.5
over 120 to 400±0.2±0.5±1.2±2.5
over 400 to 1000±0.3±0.8±2±4
over 1000 to 2000±0.5±1.2±3±6
over 2000 to 4000–±2±4±8
Permissible deviations for angular dimensions ISO 2768-1, by shorter leg
ISO 2768-1: permissible deviations for angular dimensions
shorter leg in mmf finem mediumc coarsev very coarse
up to 10±1°±1°±1°30′±3°
over 10 to 50±0°30′±0°30′±1°±2°
over 50 to 120±0°20′±0°20′±0°30′±1°
over 120 to 400±0°10′±0°10′±0°15′±0°30′
over 400±0°5′±0°5′±0°10′±0°20′

On bent parts, dimensions across a bend are coarser than cut dimensions, because sheet thickness and springback play a part. If a dimension at a bend has to be tight, specify it individually – then we check it before the quote.

Welds

Weld size and quality level

The dimension at the weld states its size – for a fillet weld, the throat thickness a. How free of imperfections it must be is set by the quality level to ISO 5817: it limits undercuts, pores, excess weld metal and other imperfections.

Fillet weld a3 in section and as a symbol on the drawing On the left a T-joint of 5 mm thick sheets in section: horizontal base plate, vertical web, in the corner the triangular fillet weld. Dimension a is the height of the triangle from the root to the weld face, here 3 mm, the leg length z about 4.2 mm. On the right the symbol: arrow line to the weld, reference line with dashed line, triangle for the fillet weld and a3 in front of it. a = 3 z ≈ 4.2 base plateweb a3 reference line dashed line: other side triangle: fillet weld, arrow side
T-joint of 5 mm sheets with fillet weld in section (a = 3 mm, leg z = a · √2) and the symbol to ISO 2553 on the drawing.
B

Stringent requirements

The tightest limits for undercuts, pores and excess weld metal – for example under high or fatigue loading. More inspection and rework time.

C

Intermediate requirements

The usual specification in steel construction and machine building when the drawing names a quality level.

D

Moderate requirements

For secondary parts where the weld only has to hold.

With stainless steel there is often a note on post-treatment as well: remove heat tint (pickling and passivation), grind welds where dirt could adhere, or “weld leak-tight” for trays and containers. For load-bearing components, EN 1090-2 refers to ISO 5817 depending on the execution class.

Examples

How it appears on the drawing

Typical specifications and what they mean for production
SpecificationMeaningFor production
√Ra 3.2 in the title blockall machined surfaces at most Ra 3.2 µmfinish cuts in turning and milling
√Ra 0.8 on one surfacethis surface at most Ra 0.8 µmgrinding or fine machining
2B, visible side grit 240 lengthwayssheet as delivered 2B, visible side ground lengthwaysgrain in one direction, protective film until assembly
⌀20 H7fitted hole, size 20.000 to 20.021 mmreaming or fine boring, checking with a plug gauge
ISO 2768-mKgeneral tolerance medium, form and position class K±0.3 mm at 100 mm
a3, fillet weld all roundthroat thickness 3 mm, all roundweld size and heat input defined
ISO 5817-Cquality level C for all weldsvisual inspection, rework for undercuts and pores
M8 – 15 deepinternal thread M8, usable 15 mm deepdrill the tap hole ⌀6.8 deeper, cut or form the thread

Upload your drawing with each part: we read surfaces, tolerances, fits, threads, press-in parts and welds for the quote and ask if a specification is missing.

Frequently asked questions

On surfaces and tolerances

Which Ra value is needed for food contact?

For surfaces in contact with the product, EHEDG recommends an arithmetic mean roughness of at most 0.8 µm. Cold-rolled stainless steel sheet 2B is usually below this as delivered; welds are ground flush, pickled and passivated so that they keep up. State on the drawing which surfaces are in contact with the product.

What does ISO 2768-mK mean?

“m” is the tolerance class medium for linear and angular dimensions to ISO 2768-1, “K” the medium class for geometrical tolerances to ISO 2768-2. A dimension of 100 mm may then deviate by ±0.3 mm. The specification applies to all dimensions that have no tolerance of their own.

Does a finer level cost more?

Yes, because work is added: grinding instead of finish cutting, reaming instead of drilling, measuring and documenting, and for welds inspection and rework. How much is stated in the quote. That is why you should specify tight values only where the part needs them.

Do you read the specifications from my drawing?

Yes. When uploading, add the drawing to each part – we evaluate surfaces, tolerances, fits, threads, rivet nuts and welds for the quote. If a specification is missing, we ask.

Unsure which level your part needs?

Describe in your request what the part is used for – we suggest the surface finish, tolerance and weld quality to match. We reply in German or English.

Free, no-obligation quote Reply within 24–48 hours on working days

Call Quote